Description
Alloy 693 is a nickel-chromium-iron-aluminum alloy with niobium addition.
Special properties
Best resistance to metal dusting in chemical and petrochemical processing environments of any conventional nickel-alloy currently manufactured.
Chemical Composition
| Cr | Fe | Cu | Ni | Ti |
| 27.0-31.0 | 2.50-6.00 | ≤0.50 | Rest | 1.00 |
| C | Si | Mn | P | S |
| ≤0.15 | ≤0.50 | ≤1.00 | ≤0.01 | ≤0.015 |
| Al | Nb | |||
| 2.5-4.0 | 0.5-2.5 |
Mechanical Properties 20℃
| 0.2% Yield strength Rp
≥N/mm2 |
Tensile strength Rm
N/mm2 |
Elongation A5
≥% |
Modulus of elasticity
kN/mm2 |
Hardness HB 30
≤HB |
| 1000 | ≥1150 | 15 | 200 | 330 |
Physical Properties 20℃
| Density
g/cm3 |
specific heat capacity
J/kg K |
Thermal conductivity W/m K | Electrical resistivity
Ω mm2/m |
| 7.77 | 475 | 16 | 1.16 |
Application
Chemical and petrochemical industry
Available forms for ALL0Y 693
Sheets/Plates
Bars
Wire
Tubes/Pipes
Fittings
Forged / cast parts
Finished part (drawing)
A grade built for one problem
Inconel 693 was developed for metal dusting — a catastrophic form of carburisation that turns steel into a mixture of metal particles and carbon in high-carbon-activity gases, typically in syngas and petrochemical reforming. It is not a general-purpose upgrade; it is a targeted answer to a specific failure.
The mechanism is compositional: about 29 % chromium with roughly 3 % aluminium forms a protective oxide that resists carbon ingress far better than the chromia on conventional alloys.
Where it is specified
- Syngas coolers and reformer outlet sections
- Petrochemical furnaces with high carbon activity
- Any location where a conventional alloy shows the pitting-and-soot signature of metal dusting
The practical point
Metal dusting is a design and operating problem as much as a material one: it is driven by carbon activity, temperature and surface condition. Changing to 693 helps, but if the gas composition and temperature put the surface in the dusting window, the alloy only buys time.
If a plant has failed with metal dusting, the useful question before ordering 693 is which of those three variables can actually be moved.
Comparing with the other grades
- Alloy 602 CA / 2.4633
- Inconel 617 / 2.4663
- Inconel 690 / N06690
- RA 333 / N06333
- Nimonic C-263 / 2.4650
- Inconel against Incoloy — which family to be in at all.
- Inconel against Incoloy — the family split.