ASTM A705 Standard Specification for Age Hardening Stainless Steel Forgings

ASTM A705 covers age-hardening stainless steel forgings — the forged counterpart of the bar specification A564. It is what you buy when the part is a forging rather than a bar: 17-4PH valve bodies, 15-5PH shafts, 17-7PH components that were forged to shape. Why there is a

Read more →

ASTM E112 2010 Standard Test Methods for Determining Average Grain Size

ASTM E112 2010 Standard Test Methods for Determining Average Grain Size Download the standard The document itself, for reference against the summary above: ASTM-E112-2010-Standard-Test-Methods-for-Determining-Average-Grain-Size (PDF)

Read more →

ASTM A580 2006 Standard Specification for Stainless Steel Wire

ASTM A580 2006 Standard Specification for Stainless Steel Wire Download the standard The document itself, for reference against the summary above: ASTM-A580-2006-Standard-Specification-for-Stainless-Steel-Wire (PDF)

Read more →

ASTM A388 Standard Practice for Ultrasonic Examination of Heavy Steel Forgings

ASTM A388 is the standard practice for ultrasonic examination of heavy steel forgings. It is a practice rather than a specification, which is the single most important thing to understand about it: it tells you how to do the test, not what you have to accept. What

Read more →

ASTM A311 Specification for cold drawn, stress relieved carbon steel bars subject to mechanical property requirements

ASTM A311 covers cold drawn, stress relieved carbon steel bars subject to mechanical property requirements. It is machining stock: bar that arrives straight, to size, with the internal stress low enough that it does not move when you cut into it. What it is for High-volume machined

Read more →

ASTM A304 2004 Standard Specification for Carbon and Alloy Steel Bars Subject to End Quench Hardenability Requirements

ASTM A304 specifies carbon and alloy steel bars by hardenability rather than by chemistry alone. It is the standard behind the “H” suffix — 4140H, 4340H, 8620H — and it exists because two heats with identical analysis can harden to different depths. What the specification actually controls

Read more →

ASTM A242 high strength low alloy structure steel

ASTM A242 is the high-strength low-alloy structural steel specified for its atmospheric corrosion resistance. It is the weathering steel of the ASTM family — the grade that forms a stable rust layer instead of continuing to corrode, which is why it is left unpainted on bridges and

Read more →

ASTM A564 2004 Standard Specification for Hot Rolled and Cold Finished Age Hardening Stainless Steel Bars and Shapes

ASTM A564 covers age-hardening (precipitation hardening) stainless steel bars, wire, shapes and forgings. It is the specification behind 17-4PH, 17-7PH and 15-5PH in bar form, and it is unusual because the same grade delivers a wide range of strengths depending on the condition it is supplied in.

Read more →

ASTM A694 Standard Specification for Carbon and Alloy Steel Forgings for Pipe Flanges, Fittings, Valves, and Parts for High-Pressure Transmission Service

ASTM A694 covers carbon and alloy steel forgings for pipe flanges, fittings, valves and parts used in high-pressure transmission service. Where A105 is the general-purpose forging grade, A694 is the one specified when the line has to carry a defined minimum yield — the F grades that

Read more →

ASTM A600 1992 Standard Specification for High Speed Tool Steel

ASTM A600 is the specification for high speed tool steel in bar form. It is the document behind a purchase order for M2, M42, T1 or any other M- and T-series high speed steel, and it is the one that decides whether the bar you receive is

Read more →

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x